this post was submitted on 31 Dec 2024
94 points (96.1% liked)

3DPrinting

15849 readers
379 users here now

3DPrinting is a place where makers of all skill levels and walks of life can learn about and discuss 3D printing and development of 3D printed parts and devices.

The r/functionalprint community is now located at: or !functionalprint@fedia.io

There are CAD communities available at: !cad@lemmy.world or !freecad@lemmy.ml

Rules

If you need an easy way to host pictures, https://catbox.moe/ may be an option. Be ethical about what you post and donate if you are able or use this a lot. It is just an individual hosting content, not a company. The image embedding syntax for Lemmy is ![](URL)

Moderation policy: Light, mostly invisible

founded 2 years ago
MODERATORS
 

Yikes. Gonna have to work with this material a bunch to learn how to use it.

Model - https://www.thingiverse.com/thing:1545913

you are viewing a single comment's thread
view the rest of the comments
[–] BigDanishGuy@sh.itjust.works 24 points 5 days ago* (last edited 5 days ago) (2 children)

First rule of PETG-club is "dry your filament", second rule of PETG-club is "dry your filament"... Thrid rule? Nope, it's "store your filament dry"

Jokes aside, other things you could look at:

  • nozzle, how worn is it?
  • calibration tests: did you do a temp tower? Calibration cube? Retraction test?
  • The vertical surface doesn't necessarily have that appearance as a result of wet filament. In my experience, wet PETG will result in more random variations than that. It looks too regular IMHO, is everything that should be tightened actually tightened?
  • have you calibrated the extruder steps?
[–] bluewing@lemm.ee 4 points 4 days ago

I would bet on retraction here. Dial that in and 90% of the stringing goes away.

[–] SzethFriendOfNimi@lemmy.world 2 points 5 days ago (3 children)

Fourth rule… painters tape as bed surface will save your PEI sheets and holds PETG really well.

Or G10/Garolite

[–] Manzas@lemdro.id 2 points 17 hours ago

Using G10 can recommend if you scratch it up you can just use the other side and if you have a metal probe you can add aluminium tape to the side you aren't using and get full functionality.

[–] bluewing@lemm.ee 5 points 4 days ago

Or just use a textured PEI plate at the proper bed temperature. There is very little need for special adjuncts to print PETG.

[–] Marvelicious@fedia.io 5 points 5 days ago

I pop my PEI bed with finished print into the freezer for about 5 minutes. Pops right off, every time. No tape, no glue, I just wash the bed with soapy water between prints.